The Difference Between a Carbon Fiber Bike Frame Repair and Wall Art by Randy Zajac I will start by saying that, in my opinion, most carbon fiber bicycle frames that have sustained damage from an impact should not be repaired—there are too many damaged fibers that are typically unseen. The two repaired frames featured in […]
Latest articles by Randy Zajac
-
-